Browsing Division of Mechanical Sciences by Subject "nanoindentation"
Now showing items 1-1 of 1
-
Understanding deformation mechanisms in the Hall-Petch breakdown regime of Ni-W alloys
The substantially higher strengths of nanocrystalline metals has been to attributed to the well-known Hall-Petch relationship σ= σ_o+k_HP d^(-1/2) where 𝜎 is the yield stress, 𝜎𝑜 is the lattice friction stress, 𝑑 is ...