Structure-Property Correlation in Additively Manufactured High-Temperature Materials: Insights from Nickel-Based Superalloy IN718 & Nickel-Based Eutectic High Entropy Alloy AlCoCrFeNi2.1
High-temperature alloys are technically very important materials that possess higher resistance toward mechanical and chemical degradation at 0.4-0.6 TM for a constant/cyclic load. These attributes make them candidate ...