Machine learning and density functional theory assisted insights into the mechanical and oxidation properties of nickel-based superalloys
Due to global warming and increasing fuel costs, there is a constant thrust toward increasing fuel efficiency and reducing the emissions of gas-turbine engines, which are made out of superalloys. New superalloy materials, ...